Name
|
Designation
|
Volume
g/cm3
|
Intensity of Cold Pressing MPa
|
Linear
Change After-Firing
|
Highest
Use Temperature ℃
|
Degree of Anti-Abrasion
CC
|
Materials
Used Parts
|
|
Abrasion-Resistant
Casting Material
|
Corundum-Quality
|
CG-B1
|
≥2.9
|
≥90
|
≥110
|
≤-0.3
|
1600
|
≤6
|
The products are
applicable to circulation vulcanized-bed boiler's
combustion chamber, return combustion belt,
water-cooling wall pipe, balanced flue, whirlwind
separator and coal spraying pipe of coal powder
furnace as abrasion and heat-resisting layer.
|